Hydrogen absorption of titaniam for nuclear waste container in non-oxidizing condition

Tomari, Haruo*; not registered; Shimogori, Kazutoshi*; Wada, Ryutaro*; not registered; Taniguchi, Naoki 

Effects of bentonite clay, applied potential, pH, of solution and cathodic polarization time on hydrogen absorption into titanium, which is one of the candidate materials of overpack for high-level radioactive waste container, have been investigated in artificial underground water. Considering the result at various test time and assuming the hydrogen absorption is ruled by the paraboric law, the amount of hydrogen after 1000 years exposure calculated to about 17ppm, which will be absorbed at the applied potential of -0.51 vs. SHE corresponds to equilibrium potential of hydrogen. It seems the assumption of the parabolic law and the test period are proper, because the linear relations were obtained between the amount of absorbed hydrogen and the logarithm of the averaged cathodic current and between the slopes of the lines and a square root of the test time. Titanium seems to have a life over 1000 years in deep underground repository according to assumption that about 500ppm absorbed hydrogen is critical for hydrogen embrittlement of titanium.

Acecsses

:

- Accesses

InCites™

:

Altmetrics

:

[CLARIVATE ANALYTICS], [WEB OF SCIENCE], [HIGHLY CITED PAPER & CUP LOGO] and [HOT PAPER & FIRE LOGO] are trademarks of Clarivate Analytics, and/or its affiliated company or companies, and used herein by permission and/or license.