Positron annihilation study of 4H-SiC by Ge$$^+$$ implantation and subsequent thermal annealing

Yu, R. S.*; Maekawa, Masaki; Kawasuso, Atsuo; Wang, B. Y.*; Wei, L.*

Positron annihilation in 800 keV Ge$$^+$$ implanted hexagonal SiC was studied by thermal annealing at temperatures ranging from 800 to 1400 $$^{circ}$$C. The variation in Doppler broadening $$S$$ values as a function of the incident positron energy suggests a broad distribution in the depth of vacancy defects in the implanted samples. Increasing the annealing temperature triggers the accumulation of vacancies into vacancy clusters. After annealing at 1400 $$^{circ}$$C, defects in the deep region of SiC are eliminated, and Ge precipitation is believed to appear in the sample at the same time. Though Ge has a much more negative positron affinity than SiC, positron annihilation coincidence Doppler broadening measurement reveals that a preferential trapping of positrons in Ge seems impossible.

Accesses

:

- Accesses

InCites™

:

Percentile:43.52

Category:Instruments & Instrumentation

Altmetrics

:

[CLARIVATE ANALYTICS], [WEB OF SCIENCE], [HIGHLY CITED PAPER & CUP LOGO] and [HOT PAPER & FIRE LOGO] are trademarks of Clarivate Analytics, and/or its affiliated company or companies, and used herein by permission and/or license.