Preperation of the charge stripping foil in J-PARC RCS

Saeki, Riuji; Yoshimoto, Masahiro  ; Yamazaki, Yoshio ; Tobita, Norimitsu; Okabe, Kota  ; Kinsho, Michikazu  ; Takeda, Osamu*; Muto, Masayoshi*

RCS has loaded with the foil of 15 sheets including a reserve into equipment so that it can exchange in a short time, when foil is damaged also in a beam operating period. It is difficult for foil to be made of a thin film about 1 micrometer thick, and to treat as it is. Then, foil is fixed to the frame which stuck the SiC fiber, and foil is not touched, but only a frame is held, and it enabled it to operate it. The following preparations are needed as new foil exchange work. (1) Exfoliation and recovery of foil which have been vapor-deposited to glass substrate. (2) Dryness and logging of exfoliative foil. (3) Preparation of SiC wire, and attachment on frame. (4) Fix foil to a frame. (5) Although charge on a magazine-rack was performed manually altogether until now, there were many work man days, and the quality of the prepared foil had variation. Then, equipment required in order to secure reproducibility was developed. The technique for working efficiently simultaneously was established. In this announcement, the technique established until now and the developed jigs are announced in detail.

Accesses

:

- Accesses

InCites™

:

Altmetrics

:

[CLARIVATE ANALYTICS], [WEB OF SCIENCE], [HIGHLY CITED PAPER & CUP LOGO] and [HOT PAPER & FIRE LOGO] are trademarks of Clarivate Analytics, and/or its affiliated company or companies, and used herein by permission and/or license.