Swelling of radiation-cured polymer precursor powder for silicon carbide by pyrolysis

Takeyama, Akinori; Idesaki, Akira; Sugimoto, Masaki; Yoshikawa, Masahito

Ceramic yield, density, volume change and pore size distribution were measured for radiation- and thermally cured (poly carbo silan) PCS powder when they were pyrolyzed in the temperature ranges between 673 and 973 K. Higher ceramic yield was obtained for radiation-cured powder due to smaller amount of evolved gas. Temperature dependence of volume change and the total pore volume show the formation and disappearance of pores in the powders were determined by the volume shrinkage and evolution of decomposed gases. Volume shrinkage narrowed the pore size distribution for radiation-cured powder. For thermally cured powder, the narrowing of size distribution was disturbed by aggregated pores. Smaller amount of evolved gas from radiation-cured powder relative to thermally cured powder prevented the aggregation of pores and provided the narrow size distribution.

Accesses

:

- Accesses

InCites™

:

Altmetrics

:

[CLARIVATE ANALYTICS], [WEB OF SCIENCE], [HIGHLY CITED PAPER & CUP LOGO] and [HOT PAPER & FIRE LOGO] are trademarks of Clarivate Analytics, and/or its affiliated company or companies, and used herein by permission and/or license.