Sorption behavior of selenide on montmorillonite

セレナイドのモンモリロナイトに対する収着挙動

杉浦 佑樹  ; 戸村 努*; 石寺 孝充 ; 土井 玲祐  ; Francisco, P. C. M.  ; 塩飽 秀啓   ; 小林 徹 ; 松村 大樹   ; 高橋 嘉夫*; 舘 幸男  

Sugiura, Yuki; Tomura, Tsutomu*; Ishidera, Takamitsu; Doi, Reisuke; Francisco, P. C. M.; Shiwaku, Hideaki; Kobayashi, Toru; Matsumura, Daiju; Takahashi, Yoshio*; Tachi, Yukio

Batch sorption experiments were performed to investigate the sorption mechanism of Se on montmorillonite under reducing conditions in deep geological environments. Based on Eh-pH diagrams and ultraviolet-visible spectra, Se was dissolved as selenide (Se(-II)) anions under the experimental conditions. The distribution coefficients ($$K_{rm d}$$; m$$^{3}$$ kg$$^{-1}$$) of Se(-II) indicated ionic strength independence and slight pH dependence. The $$K_{rm d}$$ values of Se(-II) were higher than those of Se(IV), which also exists as an anionic species. X-ray absorption near edge spectroscopy showed that the oxidation state of Se-sorbed on montmorillonite was zero even though selenide remained in the solution. These results suggest that Se(-II) was oxidized and precipitated on the montmorillonite surface. Therefore, it is implied that a redox reaction on the montmorillonite surface contributed to high $$K_{rm d}$$ values for Se(-II).

Access

:

- Accesses

InCites™

:

パーセンタイル:46.37

分野:Chemistry, Analytical

Altmetrics

:

[CLARIVATE ANALYTICS], [WEB OF SCIENCE], [HIGHLY CITED PAPER & CUP LOGO] and [HOT PAPER & FIRE LOGO] are trademarks of Clarivate Analytics, and/or its affiliated company or companies, and used herein by permission and/or license.