Effect of quenching on molten core-concrete interaction product

北垣 徹; 池内 宏知; 矢野 公彦; Brissonneau, L.*; Tormos, B.*; Domenger, R.*; Roger, J.*; 鷲谷 忠博

Journal of Nuclear Science and Technology, 56(9-10), p.902 - 914, 2019/09

AA2018-0409.pdf:2.12MB

 被引用回数:7 パーセンタイル:62.49(Nuclear Science & Technology)

Characterization of fuel debris is required to develop fuel debris removal tools. Especially, knowledge pertaining to the characteristics of molten core-concrete interaction (MCCI) product is needed because of the limited information available at present. The samples of a large-scale MCCI test performed under quenching conditions, VULCANO VW-U1, by CEA were analyzed to evaluate the characteristics of the surface of MCCI product generated just below the cooling water. As a result, the microstructure of the samples were found to be similar despite the different locations of the test sections. The Vickers hardness of each of the phases in these samples was higher than that of previously analyzed samples in another VULCANO test campaign, VBS-U4. From the comparison between analytical results of VULCANO MCCI test product, MCCI product generated under quenching condition is homogeneous and its hardness could be higher than that of the bulk MCCI product.

論文

Characterization of the VULCANO test products for fuel debris removal from the Fukushima Daiichi Nuclear Power Plant

北垣 徹; 池内 宏知; 矢野 公彦; 荻野 英樹; Haquet, J.-F.*; Brissonneau, L.*; Tormos, B.*; Piluso, P.*; 鷲谷 忠博

Progress in Nuclear Science and Technology (Internet), 5, p.217 - 220, 2018/11

Characterization of the fuel debris is required to develop fuel debris removal tools for the decommissioning of Fukushima Daiichi Nuclear Power Plant (1F). In this study, the VULCANO MCCI test, VBS-U4, was selected as 1F similar conditions and the characteristics of the samples were examined. In the molten pool sample, the round-edged corium-rich oxides region, with diameters of 1-10 mm, is surrounded by a concrete-rich oxide region. It shows convection of the molten pool. Other samples also show the features of the MCCI progression. The main chemical forms of the samples are SiO$$_{2}$$, (U,Zr)O$$_{2}$$, Fe and so on. The microstructure of the samples is heterogeneous structure composed of these phases. The difference in Vickers hardness between the metallic phases and the oxide phases is a distinctive characteristic. It can be noted that the heterogeneous distribution of metallic phases in 1F MCCI products interrupt with the removal operation such as by damaging the core-boring bit.

口頭

Characterization of fuel debris (28'A), 5; Phase and microstructure of large scale MCCI test product

北垣 徹; 池内 宏知; 矢野 公彦; 荻野 英樹; Brissonneau, L.*; Tormos, B.*; Piluso, P.*

no journal, , 

Under a collaborative agreement with CEA, the phases and microstructures of large-scale MCCI test products from PLINIUS/VULCANO experiments have been analyzed. The phases and microstructures vary at different sampling locations, each of which is representative of a product to be generated under severe accident conditions and which is considered to be close to that of Fukushima Daiichi Nuclear Power Station Unit 1.