Benchmark analysis by Beremin model and GTN model in CAF subcommittee

廣田 貴俊*; 名越 康人*; 北条 公伸*; 岡田 裕*; 高橋 昭如*; 勝山 仁哉; 上田 貴志*; 小川 琢矢*; 八代醍 健志*; 大畑 充*; et al.

Proceedings of ASME 2021 Pressure Vessels and Piping Conference (PVP 2021) (Internet), 9 Pages, 2021/07

In order to establish a guideline for fracture evaluation by considering plastic constraint in the ductile-brittle transition temperature (DBTT) region, the CAF (Constraint-Based Assessment of Fracture in Ductile-Brittle Transition Temperature Region) subcommittee has been launched in 2018 in the Japan Welding Engineering Society. In the committee, fracture tests are conducted using C(T), SE(B), and 50mm-thick flat plate with a surface flaw subjected to bending load or tensile load to verify fracture evaluation methods. Since simulation results are easily affected by analysis conditions, benchmark analysis is essential for the potential users of the guideline. Therefore, benchmark analyses are executed on brittle and ductile damages by Beremin and Gurson-Tvergaard-Needleman (GTN) models implemented in the finite element (FE) codes. The benchmark analyses are carried out in four steps; Step 0 is to confirm the output of FE codes in each member with the same input data and the same FE model. Step 1 is to confirm the result of Weibull stress analysis for C(T) specimens tested at -125$$^{circ}$$C. The Weibull parameter, m, was fixed in this step. At step 2, sensitivity analyses are conducted on Weibull stresses in different conditions. The outputs by the GTN model are also confirmed. At the final step, the fracture simulation will be run for flat plate specimens with less plastic constraint than the standard fracture toughness specimen. As the results of the benchmark analyses up to step 2, a significant difference is not observed in the Weibull stress computed by committee members with the same input data and FE model and it is confirmed that the effects of element type, nonlinear deformation theory employed in FE analysis. For the calculation of the Weibull parameter m by using the fracture toughness test results and the developed programs by committee members, the converged values of m show good agreement among them.

論文

Benchmark analyses of probabilistic fracture mechanics for cast stainless steel pipe

北条 公伸*; 林 翔太郎*; 西 亘*; 釜谷 昌幸*; 勝山 仁哉; 眞崎 浩一*; 永井 政貴*; 岡本 年樹*; 高田 泰和*; 吉村 忍*

Mechanical Engineering Journal (Internet), 3(4), p.16-00083_1 - 16-00083_16, 2016/08

鋳造ステンレス鋼に対する非破壊検査が計画されているが、鋳造ステンレス鋼のような二相ステンレス鋼では、超音波の低い透過性などの理由から、許容欠陥寸法が定められていない。鋳造ステンレス鋼の許容欠陥寸法を合理的に決定するためには、確率論的破壊力学(PFM)は有用である。本研究では、鋳造ステンレス鋼配管を対象に、PFM解析コードの適用性や信頼性に係るベンチマーク問題を提案した。破損モードとしては、疲労亀裂進展、塑性崩壊、及び延性亀裂進展を考慮し、それらの相互作用を考慮した条件でPFM解析を行った。6機関が参加して実施されたベンチマーク解析による破損確率の比較を行った。その結果、各機関で様々なPFM解析コードで得られた破損確率はよく一致し、鋳造ステンレス鋼配管に対するPFMの適用性が確認された。

論文

Elaboration of the system based code concept; Activities in JSME and ASME, 2; Development of evaluation tools based on LRFD

町田 秀夫*; 浅山 泰; 渡辺 大剛*; 北条 公伸*; 林 正明*

Proceedings of 22nd International Conference on Nuclear Engineering (ICONE-22) (DVD-ROM), 10 Pages, 2014/07

本論文は、原子力プラントの構造規格基準への適用を目指して開発が進められているシステム化規格概念に関する日本機械学会(JSME)および米国機械学会(ASME)における活動について述べた4件のシリーズ発表の第2報である。本報では、高速炉の静的機器に対する構造信頼性評価法を、土木・建築分野では実用化例のある荷重・耐力係数設計法(LRFD)に基づいて開発した結果について述べる。