土屋 朋生*; 小林 亮太*; 窪田 崇秀*; 斉藤 耕太郎*; 小野 寛太*; 大原 高志; 中尾 朗子*; 高梨 弘毅*
Journal of Physics D; Applied Physics, 51(6), p.065001_1 - 065001_7, 2018/02
被引用回数:8 パーセンタイル:46.45(Physics, Applied)MnVAl Heusler alloy films were epitaxially grown on MgO(100) single-crystal substrates by ultra-high-vacuum magnetron sputtering. A2- and L21-type MnVAl order was controlled by the deposition temperature. A2-type MnVAl films showed no spontaneous magnetization, while L21-type MnVAl films showed ferrimagnetic behaviour with a maximum saturation magnetization of 220 emu/cm at room temperature (RT). An antiferromagnetic reflection was observed with neutron diffraction at RT for an A2-type MnVAl film deposited at 400C. A bilayer sample of the antiferromagnetic A2-type MnVAl and Fe showed an exchange bias of 120 Oe at 10 K.
小林 理気*; 金子 耕士; 斉藤 耕太郎*; Mignot, J.-M.*; Andr, G.*; Robert, J.*; 脇本 秀一; 松田 雅昌*; Chi, S.*; 芳賀 芳範; et al.
Journal of the Physical Society of Japan, 83(10), p.104707_1 - 104707_5, 2014/10
被引用回数:16 パーセンタイル:68.66(Physics, Multidisciplinary)The effect of electron doping by the substitution of Rh for Ru on unconventional magnetic order in CeRuAl was investigated via neutron powder diffraction. In Ce(RuRh)Al with = 0.05, 0.12, 0.2, reorientation of the ordered moment from the - to the -axis takes place in all samples, while the ordering vector = (0 1 0) remains unchanged within this concentration range. The moment reorientation is accompanied by an enhancement in its size by a factor of 2.4, from =0.43 at = 0 to =1.06, 1.04, and 1.02 for = 0.05, 0.12 and 0.2, respectively. The continuous decrease in Nel temperature (), despite an abrupt increase in , underlines the strong anisotropy in the exchange interaction in CeRuAl, and the fact that this anisotropy is easily suppressed by electron doping.