中性子回折によるフェライト単相鋼のひずみ時効硬化異方性の検討

鈴木 徹也*; 山中 啓輔*; 石野 まゆ子*; 篠原 康浩*; 長井 健介*; 津留 英司*; 徐 平光

鉄と鋼, 98(6), p.262 - 266, 2012/06

The work-hardening characteristics of anisotropic tensile deformations and the corresponding residual strain changes of pre-strained ferritic steels without and with ageing treatment were investigated by using angle dispersive neutron diffraction and electron back-scattering diffraction. The plastic deformation along the pre-strained direction leads to evident work-hardening at the beginning stage, showing discontinuous yielding behavior. Comparably, the plastic deformation perpendicular to the pre-strained direction shows continuously yielding. The tensile and compressive residual strains were found in the $$<$$200$$>$$ and $$<$$110$$>$$ grains along the pre-strained direction, respectively. It is also found that the difference in various oriented grains after strain ageing become more evident along the pre-strained direction but smaller perpendicular to the pre-strained direction, revealing a higher work hardening capability in the former case than in the latter case.

口頭

ひずみ時効硬化特性の方位依存性評価

鈴木 徹也*; 山中 啓輔*; 石野 まゆ子*; 徐 平光; 鈴木 裕士

no journal, , 

フェライト単相鋼材の予ひずみ方向がその後の時効硬化挙動にどのような影響を与えるか調査した。特に結晶方位による塑性異方性に注目し、予ひずみにより導入される加工の結晶方位依存性、その後の引張り変形における結晶方位群ごとの残留ひずみを中性子回折により測定した。また、EBSPにより変形に伴う組織の変化を時効前後について解析した。結果としては、結晶方位ごとに残留ひずみの値が異なり、200粒に引張りの残留ひずみが存在することが分かる。ひずみが大きくなるほどKernel平均方位差(KAM)値が増加している。時効前の試料は200粒のKAM値の増加率が110粒よりも大きい。ひずみ時効後の試料のKAM値の増加率は、110粒は時効前の試料とほぼ変わらないが、200粒はひずみ4%までは時効前の200粒より大きい。このことは時効硬化後の塑性変形挙動にKAM値に影響を与えるような結晶粒異方性が存在することを意味する。