上路 林太郎*; Gong, W.; Harjo, S.; 川崎 卓郎; 柴田 曉伸*; 木村 勇次*; 井上 忠信*; 土田 紀之*
ISIJ International, 64(2), p.459 - 465, 2024/01
被引用回数:4 パーセンタイル:36.86(Metallurgy & Metallurgical Engineering)Deformation-induced martensitic transformation (DIMT) during tensile or compressive deformations of the bainitic steels with various carbon content (0.15%C, 0.25%C, 0.62%C) was studied. In all of the bainitic steels, the tensile deformation exhibited larger work hardening than the compression. This difference indicates the suppression of the DIMT at the compression, and actually the measurements of electron back scattering diffraction (EBSD) confirmed the less reduction of retained austenite at the compression of all the bainitic steels. Additionally, the steel with the highest carbon content was examined by in situ neutron diffraction and clarified the difference similar to that obtained by the EBSD measurement. The regression of the relation between the fraction of austenite and applied strain with the conventional empirical equation revealed that the kinetic of DIMT is strongly dependent with the stress polarity, but not significantly changed by the carbon content.
土田 紀之*; Kuramoto, Shota*; 上路 林太郎*; Gong, W.; Harjo, S.; 廣井 孝介; 河村 幸彦*
ISIJ International, 64(2), p.354 - 360, 2024/01
被引用回数:0 パーセンタイル:0.00(Metallurgy & Metallurgical Engineering)The effects of pre-strain on the mechanical properties of high strength martensitic steels were investigated using either strain tempering (ST) or quenching and tempering (QT) samples. In the tensile tests at deformation temperatures between 296 and 573 K, the ST sample exhibited an increase in both the tensile strength (TS) and uniform elongation (U El) at 473 to 523 K, whereas the QT sample showed an increase in U El with little change in the TS and yield strength (YS). The results of in situ neutron diffraction experiments revealed an increase in the stress partitioning to the bcc phase with an increase in the deformation temperature from 296 to 523 K. The difference in the phase stress between the bcc and cementite phases decreased with an increase in the temperature due to the decrease in the cementite strength. Pre-strain of 0.5% increased the YS at 296 K with a slight work hardening; the initial dislocation density (
) decreased at 523 K, but increased significantly after yielding, leading to a better combination of TS and U.El. The combination of pre-strain, tempering, and deformation temperatures caused the change in
before deformation and the increase in
after yielding of the martensitic steel.
土田 紀之*; 上路 林太郎*; Gong, W.; 川崎 卓郎; Harjo, S.
Scripta Materialia, 222, p.115002_1 - 115002_6, 2023/01
被引用回数:12 パーセンタイル:47.40(Nanoscience & Nanotechnology)The present study investigated the tensile deformation behavior of quenched and tempered martensite steels at various austenitization and tempering temperatures using in situ neutron diffraction experiments. Phase lattice strains in the bcc and cementite (
) phases and dislocation structures in the bcc phase were analyzed. The phase lattice strain in bcc became almost stagnant after yielding as the tempering temperature increased. The phase lattice strain in
increased linearly with an increase in the flow stress, independent of the austenitization and tempering temperatures. The stress partitioning between bcc and
was confirmed after the yielding of bcc, which contributed to the work hardening. The phase stresses of bcc and
and their stress partitioning improve the mechanical properties of martensite steels, which can be summarized by the systematic changes in phase lattice strain and dislocation properties due to the austenitization and tempering temperatures.