論文

Neutron diffraction monitoring of ductile cast iron under cyclic tension-compression

Harjo, S.; 窪田 哲*; Gong, W.*; 川崎 卓郎; Gao, S.*

Acta Materialia, 196, p.584 - 594, 2020/09

 被引用回数:0 パーセンタイル:100(Materials Science, Multidisciplinary)

To understand work hardening behavior during low-cycle loading, ductile cast iron containing spheroidal graphite, pearlite, and ferrite matrix was investigated in an in situ neutron diffraction study of up to four cycles of tensile-compressive loading with applied strains of $$pm$$0.01. The amplitudes of applied stress, Bauschinger stress, and Bauschinger strain were found to increase with increasing cycle number, indicating work hardening as cyclic loading progressed. Absolute values of ferrite lattice strain at maximum and minimum applied strains increased with increasing cycle number, indicating an increase in ferrite strength. Consequently, the stress contribution to the strength from ferrite increased as cyclic loading progressed. The increase in ferrite strength, caused by dislocation accumulation in ferrite during cyclic loading, played an important role in the work hardening of the ductile cast iron.

論文

沸騰硫酸中における鉄-シリコン合金の耐食性と表面皮膜の性状

井岡 郁夫; 森 順二*; 加藤 千明; 二川 正敏; 小貫 薫

日本金属学会誌, 63(5), p.609 - 612, 1999/00

高シリコン鋳鉄は、硫酸中で良好な耐食性を示す。耐食性の発現機構を調べるため、沸騰硫酸下で生成したFe-Si合金の耐食皮膜の特性を調べた。試験片は、Fe-20%Si合金を用い、50%及び95%の沸騰硫酸に浸せきした。50%硫酸の皮膜表面は金属光沢を、95%硫酸では金属光沢のない黒褐色を示した。オージェ電子分光法により、皮膜の組成は50%硫酸ではSiとO、95%硫酸ではSi,O,Sから成ることがわかった。皮膜の生成速度は、95%硫酸の方が50%硫酸より一桁程度速かった。また、X線光電子分光法により50%硫酸の皮膜はSiO$$_{2}$$であり、95%硫酸の皮膜はSiO$$_{2}$$とSiOであることがわかった。95%硫酸の皮膜中のSは分子状のままで存在する硫酸分子のSへの還元反応により生成されたもの、被膜の生成速度の違いは被膜自体の緻密さによるものと考えられる。