JAEA Reports

Development of zeolite column adsorption dynamics simulation code (ZAC)

Yamagishi, Isao; Hato, Shinji*; Nishihara, Kenji; Tsubata, Yasuhiro; Sagawa, Yusuke*

JAEA-Data/Code 2024-002, 63 Pages, 2024/07

JAEA-Data-Code-2024-002.pdf:2.91MB
JAEA-Data-Code-2024-002-appendix(CD-ROM).zip:9.42MB

Adsorption columns filled with zeolite are used to treat contaminated water containing radioactive cesium generated by the Fukushima Daiichi Nuclear Power Station accident. As the contaminated water treatment progresses, the radioactive cesium in the adsorption column becomes highly concentrated, and the adsorption column becomes a high radiation source. To evaluate the radiation effects such as decay heat and radiolytic hydrogen production in the adsorption column, the concentration of radioactive cesium in the adsorption column is necessary, but since it is difficult to evaluate the concentration by measurement, it is estimated by simulation. In this research, a zeolite column adsorption dynamics simulation (Zeolite Adsorption Column: ZAC) code was developed to calculate the concentration of radioactive materials such as radioactive cesium in a zeolite filled adsorption column when they are injected into the column. The code was validated through comparison of calculation results with existing codes and experimental results of small column tests. This report presents the details of the model, the handling of the code, and the validity of the results for the developed code.

Journal Articles

Cohesive/Adhesive strengths of CsOH-chemisorbed SS304 surfaces

Li, N.*; Sun, Y.*; Nakajima, Kunihisa; Kurosaki, Ken*

Journal of Nuclear Science and Technology, 61(3), p.343 - 353, 2024/03

 Times Cited Count:1 Percentile:0.00(Nuclear Science & Technology)

During the Fukushima Daiichi nuclear power plant (1F) accident, an overwhelming amount of the cesium remaining in the pressure vessel could have been deposited onto 304 stainless steel (SS304) steam separators and dryers, both with large surface areas. During 1F's decommissioning, the deposited cesium is a safety hazard as it can generate radioactive dust. However, the cohesive and adhesive strengths of CsOH-chemisorbed oxide scales are yet to be defined. In this study, we investigated how CsOH-chemisorption affects the cohesive and adhesive strengths between oxide scales and SS304 substrates with a scratch tester. The scratch test results revealed that the cohesive strengths of the oxide scales decreased after CsOH-chemisorption, while adhesive failure could not be reached.

Journal Articles

Effects of gamma-ray irradiation on spontaneous potential of stainless steel in zeolite-containing diluted artificial seawater

Kato, Chiaki; Sato, Tomonori; Ueno, Fumiyoshi; Yamagishi, Isao

Proceedings of 17th International Conference on Environmental Degradation of Materials in Nuclear Power Systems - Water Reactors, Vol.2, p.1357 - 1374, 2016/05

With respect to the long-term storage of the zeolite-containing spent Cs adsorption vessels used at the Fukushima Daiichi Nuclear Power Station, the corrosion of the vessel material is one of the most important issues. In this study, we performed electrochemical tests on stainless steel specimens in zeolite-containing artificial seawater under gamma-ray irradiation. The spontaneous potential ESP and critical pitting potential VC of the type 316L steel in systems in contact with various zeolites were measured in order to evaluate the corrosion resistance of the steel. In addition, the water sample was analyzed after being irradiated, in order to determine the concentrations of various dissolved oxidants such as oxygen and hydrogen peroxide, which can accelerate the corrosion process. The steady-state rest potential increased with an increase in the dose rate; however, the increase was suppressed in contact with the zeolites. The VC value of the steel when in contact with the zeolites was slightly smaller than the VC value in bulk water; however, the choice of the zeolite used as herschelite, IE96 and IE911 hardly affect the VC value. The concentration of H$$_{2}$$O$$_{2}$$ in the bulk water under irradiation also increased with the increase in the dose rate. This increase was suppressed in the systems in contact with the zeolites, owing to the decomposition of the H$$_{2}$$O$$_{2}$$ by the zeolites. A clear relationship was observed between ESP and the H$$_{2}$$O$$_{2}$$ concentration. As contact with the zeolites caused the increase in ESP under irradiation to be suppressed, it can be concluded that the presence of zeolites in the spent Cs adsorption vessels can reduce the probability of the localized corrosion of the stainless steel in the vessels.

Journal Articles

Cesium-adsorption behavior of weathered biotite from Fukushima Prefecture depends on the degree of vermiculitization

Yamada, Hirohisa*; Yokoyama, Shingo*; Watanabe, Yujiro*; Suzuki, Masaya*; Suzuki, Shinichi; Hatta, Tamao*

Nihon Ion Kokan Gakkai-Shi, 25(4), p.207 - 211, 2014/11

JAEA Reports

Removal of radionuclides from partitioning waste solutions by adsorption and catalytic oxidation methods

Yamagishi, Isao; Yamaguchi, Isoo; Kubota, Masumitsu*

JAERI-Research 2000-038, 40 Pages, 2000/09

JAERI-Research-2000-038.pdf:1.33MB

no abstracts in English

Journal Articles

Adsorption and desorption characteristics of silver on the borosilicate glass surface

Sato, Tadashi

Radiochimica Acta, 46, p.101 - 108, 1989/00

no abstracts in English