Refine your search:     
Report No.
 - 

Main results of static and dynamic corrosion tests in oxygen-saturated liquid lead-bismuth

Kurata, Yuji; Kikuchi, Kenji; Saito, Shigeru   ; Futakawa, Masatoshi  ; Sasa, Toshinobu   

A report at MEGAPIE(Megawatt Pilot Experiment) Technical R & D Meeting is collected into an FZK report. According to the static corrosion tests, Al surface-treated layer produced by the gas diffusion method exhabited corrosion resistance to liquid Pb-Bi, while Al surface-treated layer produced by the melt dipping method suffered a severe corrosion attack. Furtheremore, it was found that a thick ferrite layer was formed in the surface of austenitic stainless steel at 550$$^{circ}$$C. Dissolution at high temperature parts, precipitation of Fe-Cr alloy and deposition of PbO at low temperature parts occured in the first loop corrosion test. These caused plugging of the narrow passage in electro-magnetic pumu(EMP) system. Adoption of filters and a wide passage in an EMP system, and the use of an inner-polished tube specimen brought about a good effect.

Accesses

:

- Accesses

InCites™

:

Altmetrics

:

[CLARIVATE ANALYTICS], [WEB OF SCIENCE], [HIGHLY CITED PAPER & CUP LOGO] and [HOT PAPER & FIRE LOGO] are trademarks of Clarivate Analytics, and/or its affiliated company or companies, and used herein by permission and/or license.