${it Ex-situ}$ and ${it in-situ}$ X-ray diffractions of corrosion products freshly formed on the surface of an iron-silicon alloy

Suzuki, Shigeru*; Matsubara, Eiichiro*; Komatsu, Takuya*; Okamoto, Yoshinori*; Kanie, Kiyoshi*; Muramatsu, Atsushi*; Konishi, Hiroyuki; Mizuki, Junichiro; Waseda, Yoshio*

${it Ex-situ}$ X-ray diffraction measurements of a small amount of samples extracted from wet corrosion products freshly formed on a pure iron and iron-2 mass% silicon surfaces have been conducted using synchrotron radiation. The results showed that $$gamma$$-FeOOH was formed on the outer side of wet corrosion products formed on the pure iron by sodium chloride solution, while $$gamma$$-FeOOH, $$alpha$$-FeOOH, Fe$$_{3}$$O$$_{4}$$, and green rusts were formed on the inner side. In comparison to the case of the pure iron, a significant formation of $$beta$$-FeOOH was observed in the iron-silicon alloy. Furthermore, in-situ diffraction measurements by a conventional X-ray source were conducted for analyzing corrosion products formed on the pure iron and iron-silicon alloy surfaces by cyclic exposure to wet and dry atmospheres. The results obtained by the ${it in-situ}$ diffraction and ${it ex-situ}$ diffraction measurements on the corrosion products were consistent.

Accesses

:

- Accesses

InCites™

:

Percentile:80.42

Category:Materials Science, Multidisciplinary

Altmetrics

:

[CLARIVATE ANALYTICS], [WEB OF SCIENCE], [HIGHLY CITED PAPER & CUP LOGO] and [HOT PAPER & FIRE LOGO] are trademarks of Clarivate Analytics, and/or its affiliated company or companies, and used herein by permission and/or license.