Influence of boron vapor on transport behavior of deposited CsI during heating test simulating a BWR severe accident condition

Sato, Isamu; Onishi, Takashi  ; Tanaka, Kosuke  ; Iwasaki, Maho; Koyama, Shinichi  

We observed one of the simplified processes by conducting primitive experiments. CsI was heated at 1323 K to be vaporized and deposited on sampling parts with a temperature range of 1023 - 423 K and then B$$_{2}$$O$$_{3}$$ was vaporized at 1973 K to be reacted with Cs/I there. After heating tests, each sampling part was soaked into alkali water to dissolve the surface-deposits for ICP-MS analysis. The results showed that CsI deposited at the sampling parts kept above approx. 850 K was striped by B$$_{2}$$O$$_{3}$$ vapour. This behaviour will be thermodynamically discussed to study the Cs/I/B chemistry in the severe accidents.

Accesses

:

- Accesses

InCites™

:

Altmetrics

:

[CLARIVATE ANALYTICS], [WEB OF SCIENCE], [HIGHLY CITED PAPER & CUP LOGO] and [HOT PAPER & FIRE LOGO] are trademarks of Clarivate Analytics, and/or its affiliated company or companies, and used herein by permission and/or license.