Strain hardening behavior of additively manufactured and annealed AlSi3.5Mg2.5 alloy

金属積層造形および焼きなまし処理されたAlSi3.5Mg2.5合金の加工硬化挙動

Zhang, X. X.*; Lutz, A.*; Andr$"a$, H.*; Lahres, M.*; Gong, W.   ; Harjo, S.   ; Emmelmann, C.*

Zhang, X. X.*; Lutz, A.*; Andr$"a$, H.*; Lahres, M.*; Gong, W.; Harjo, S.; Emmelmann, C.*

The ductility of the Al alloys produced by additive manufacturing (AM) has become a critical property, as the AM Al alloys are increasingly used in the automotive industry. However, the ductility of as-built AM Al alloys is relatively low, even with optimized AM conditions. The post-annealing treatment provides an efficient way to improve ductility. Previous investigation has shown that the annealed AM AlSi3.5Mg2.5 alloy possesses superior ductility. However, the plastic deformation micro-mechanisms of the annealed AM AlSi3.5Mg2.5 alloy remain unclear. In this study, in-situ neutron diffraction was employed to explore the annealed AM AlSi3.5Mg2.5 alloy. The evolutions of phase stresses, dislocation density, and crystallite size in the annealed AM AlSi3.5Mg2.5 alloy during tensile deformation were analyzed. The experimental investigation reveals that the dislocation density in the Al matrix of the annealed AM AlSi3.5Mg2.5 alloy increases slowly in the early plastic deformation stage, and it reaches a saturated level upon the following uniform deformation. The crystallite size decreases quickly in the early deformation stage, and then it decreases slowly. The Kocks-Mecking model and the Voce model can capture the strain hardening behavior well. The determined physical constitutive equations can be applied in continuum mechanical computer simulations.

Access

:

- Accesses

InCites™

:

パーセンタイル:71.08

分野:Chemistry, Physical

Altmetrics

:

[CLARIVATE ANALYTICS], [WEB OF SCIENCE], [HIGHLY CITED PAPER & CUP LOGO] and [HOT PAPER & FIRE LOGO] are trademarks of Clarivate Analytics, and/or its affiliated company or companies, and used herein by permission and/or license.